Flexural Strength of Modern CAD/CAM Restoratives After Artificial Aging.

Melc 2024 · Melc Thomas, Attin Thomas, Eyüboğlu Tan Fırat, et al. · Materials (Basel, Switzerland) · 2024

Included by

Outcome this study informsPooled effectEvidenceCertainty
Flexural strength
Thermocycling and/or artificial aging vs Non-aged control or baseline specimens · After aging protocol
SMD -1.68 [-2.73, -0.62]5 studiesGRADE not reported
Flexural strength
Thermocycling and/or artificial aging vs Non-aged control or baseline specimens · After aging protocol
SMD -1.68 [-2.28, -1.08]5 studies · 404 participantsGRADE not reported
Flexural strength
Thermocycling and/or artificial aging vs Non-aged control or baseline specimens · After aging protocol
SMD -1.495 studiesGRADE not reported
Flexural strength
Thermocycling and/or artificial aging vs Non-aged control or baseline specimens · After aging protocol
SMD -1.845 studiesGRADE not reported