Prior SDF application with a rinsing step vs No prior SDF application (untreated dentin control)
Immediate bond strength (MPa) · Dental adhesives bonded to caries-affected dentin (in vitro)
Prior SDF followed by a rinsing step significantly increases adhesive bond strength to caries-affected dentin (MD -4.79 MPa favoring SDF, 95% CI -9.19 to -0.40; ungraded).
1 finding from 1 review
- Bonding of Glass-Ionomer Cement and Adhesives to Silver Diamine Fluoride-treated Dentin: An Updated Systematic Review… 2022 All outcomesImmediate bond strength · In vitro (laboratory bond-strength testing) · Caries-affected dentin (with rinsing step)MD -4.79 [-9.19, -0.40]3 studies · 72 participantsGRADE not reported