Hydroxyapatite (e.g., nano-HAp) vs Calcium phosphate agent (e.g., CPP-ACP, Ca/P-PILP, niobophosphate)

Immediate (24 h) resin-dentin bond strength (MPa) · Artificial caries-affected dentin (ACAD) in extracted permanent human teeth (in vitro)

In the Self-Etch adhesive + chemical ACAD protocol network, HAp showed 4.455 MPa lower 24 h bond strength than Calcium Phosphate (MD -4.455, 95% CI -8.857 to -0.053; Moderate certainty).

2 findings from 1 review

Self-assembling/remineralizing peptide (e.g., P11-4, PAA-PASP) vs Flavonoids (e.g., quercetin, proanthocyanidin)

Immediate (24 h) resin-dentin bond strength (MPa) · Artificial caries-affected dentin (ACAD) in extracted permanent human teeth (in vitro)

In the Etch-and-Rinse adhesive + biological ACAD protocol network, Peptide showed 9.857 MPa higher 24 h bond strength than Flavonoids (MD 9.857, 95% CI 2.588 to 17.126; Moderate certainty).

2 findings from 1 review

Mesoporous silica (SiO2) vs Calcium phosphate agent (e.g., CPP-ACP, Ca/P-PILP, niobophosphate)

Immediate (24 h) resin-dentin bond strength (MPa) · Artificial caries-affected dentin (ACAD) in extracted permanent human teeth (in vitro)

In the Self-Etch adhesive + chemical ACAD protocol network, Silica vs Calcium Phosphate showed no significant difference in 24 h bond strength (MD -0.699, 95% CI -7.633 to 6.234; Moderate certainty).

1 finding from 1 review

Calcium phosphate agent (e.g., CPP-ACP, Ca/P-PILP, niobophosphate) vs No biomimetic remineralization (control)

Immediate (24 h) resin-dentin bond strength (MPa) · Artificial caries-affected dentin (ACAD) in extracted permanent human teeth (in vitro)

In the Self-Etch adhesive + chemical ACAD protocol network, Calcium Phosphate vs Control showed no significant difference in 24 h bond strength (MD 1.539, 95% CI -1.738 to 4.817; Moderate certainty).

1 finding from 1 review

HEMA/EGDMA-based desensitizer vs Fluoride agent (e.g., NaF/SDF/KF/CaF2)

Immediate (24 h) resin-dentin bond strength (MPa) · Artificial caries-affected dentin (ACAD) in extracted permanent human teeth (in vitro)

In the Self-Etch adhesive + chemical ACAD protocol network, HEMA vs Fluorine showed no significant difference in 24 h bond strength (MD 2.500, 95% CI -2.603 to 7.603; Low certainty).

1 finding from 1 review

Flavonoids (e.g., quercetin, proanthocyanidin) vs Calcium-based agent

Immediate (24 h) resin-dentin bond strength (MPa) · Artificial caries-affected dentin (ACAD) in extracted permanent human teeth (in vitro)

In the Self-Etch adhesive + chemical ACAD protocol network, Flavonoids vs Calcium showed no significant difference in 24 h bond strength (MD 5.728, 95% CI -2.442 to 13.897; Moderate certainty).

1 finding from 1 review

Hydroxyapatite (e.g., nano-HAp) vs Flavonoids (e.g., quercetin, proanthocyanidin)

Immediate (24 h) resin-dentin bond strength (MPa) · Artificial caries-affected dentin (ACAD) in extracted permanent human teeth (in vitro)

In the Self-Etch adhesive + chemical ACAD protocol network, HAp showed 7.520 MPa lower 24 h bond strength than Flavonoids (MD -7.520, 95% CI -14.758 to -0.281; Moderate certainty).

1 finding from 1 review

Mesoporous silica (SiO2) vs HEMA/EGDMA-based desensitizer

Immediate (24 h) resin-dentin bond strength (MPa) · Artificial caries-affected dentin (ACAD) in extracted permanent human teeth (in vitro)

In the Self-Etch adhesive + chemical ACAD protocol network, Silica vs HEMA showed no significant difference in 24 h bond strength (MD -1.059, 95% CI -9.024 to 6.906; Moderate certainty).

1 finding from 1 review

Calcium-based agent vs No biomimetic remineralization (control)

Immediate (24 h) resin-dentin bond strength (MPa) · Artificial caries-affected dentin (ACAD) in extracted permanent human teeth (in vitro)

In the Self-Etch adhesive + chemical ACAD protocol network, Calcium vs Control showed no significant difference in 24 h bond strength (MD -1.124, 95% CI -5.917 to 3.670; Moderate certainty).

1 finding from 1 review

Flavonoids (e.g., quercetin, proanthocyanidin) vs Mesoporous silica (SiO2)

Immediate (24 h) resin-dentin bond strength (MPa) · Artificial caries-affected dentin (ACAD) in extracted permanent human teeth (in vitro)

In the Self-Etch adhesive + chemical ACAD protocol network, Flavonoids vs Silica showed no significant difference in 24 h bond strength (MD 3.764, 95% CI -5.241 to 12.769; Moderate certainty).

1 finding from 1 review