Mesoporous silica (SiO2) vs Calcium-based agent
Immediate (24 h) resin-dentin bond strength (MPa) · Artificial caries-affected dentin (ACAD) in extracted permanent human teeth (in vitro)
In the Self-Etch adhesive + chemical ACAD protocol network, Silica vs Calcium showed no significant difference in 24 h bond strength (MD 1.964, 95% CI -5.802 to 9.730; Moderate certainty).
1 finding from 1 review
- Biomimetic Remineralization Strategies for Dentin Bond Stability-Systematic Review and Network Meta-Analysis. 2025 All outcomes24 h (immediate) · In vitro; extracted permanent human teeth; bond strength testing (SBS/microSBS/microTBS) · Self-Etch + chemical ACADMD 1.964 [-5.802, 9.730]0 studiesModerate