Immediate (24 h) resin-dentin bond strength (MPa) · permanent human teeth with artificial caries-affected dentin
Calcium phosphate minus Control was -21.209 MPa (95% CI -25.954 to -16.463) at 24 h.
2 findings from 1 review
MD -21.209 [-25.954, -16.463]
2 studies
Moderate
MD -1.105 [-4.828, 2.619]
1 study
Low
Immediate (24 h) resin-dentin bond strength (MPa) · Artificial caries-affected dentin (ACAD) in extracted permanent human teeth (in vitro)
In the Etch-and-Rinse adhesive + biological ACAD protocol network, Flavonoids showed 8.438 MPa higher 24 h bond strength than Control (MD 8.438, 95% CI 2.289 to 14.587; Moderate certainty).
2 findings from 1 review
Immediate (24 h) resin-dentin bond strength (MPa) · Artificial caries-affected dentin (ACAD) in extracted permanent human teeth (in vitro)
In the Self-Etch adhesive + chemical ACAD protocol network, HEMA vs Calcium showed no significant difference in 24 h bond strength (MD 3.023, 95% CI -3.815 to 9.861; Moderate certainty).
1 finding from 1 review
Immediate (24 h) resin-dentin bond strength (MPa) · Artificial caries-affected dentin (ACAD) in extracted permanent human teeth (in vitro)
In the Self-Etch adhesive + chemical ACAD protocol network, Peptide vs HEMA showed no significant difference in 24 h bond strength (MD -0.369, 95% CI -6.728 to 5.990; Low certainty).
1 finding from 1 review
Immediate (24 h) resin-dentin bond strength (MPa) · Artificial caries-affected dentin (ACAD) in extracted permanent human teeth (in vitro)
In the Self-Etch adhesive + chemical ACAD protocol network, HAp vs Control showed no significant difference in 24 h bond strength (MD -2.916, 95% CI -5.854 to 0.023; Moderate certainty).
2 findings from 1 review
Immediate (24 h) resin-dentin bond strength (MPa) · Artificial caries-affected dentin (ACAD) in extracted permanent human teeth (in vitro)
In the Self-Etch adhesive + chemical ACAD protocol network, HEMA vs Calcium Phosphate showed no significant difference in 24 h bond strength (MD 0.360, 95% CI -5.589 to 6.309; Moderate certainty).
1 finding from 1 review
Immediate (24 h) resin-dentin bond strength (MPa) · Artificial caries-affected dentin (ACAD) in extracted permanent human teeth (in vitro)
In the Etch-and-Rinse adhesive + chemical ACAD protocol network, HAp vs Fluorine showed no significant difference in 24 h bond strength (MD 4.960, 95% CI -1.806 to 11.727; Low certainty).
2 findings from 1 review
Immediate (24 h) resin-dentin bond strength (MPa) · Artificial caries-affected dentin (ACAD) in extracted permanent human teeth (in vitro)
In the Self-Etch adhesive + chemical ACAD protocol network, Flavonoids vs HEMA showed no significant difference in 24 h bond strength (MD 2.705, 95% CI -5.654 to 11.063; Moderate certainty).
1 finding from 1 review
Immediate (24 h) resin-dentin bond strength (MPa) · Artificial caries-affected dentin (ACAD) in extracted permanent human teeth (in vitro)
In the Self-Etch adhesive + chemical ACAD protocol network, Silica vs Control showed no significant difference in 24 h bond strength (MD 0.840, 95% CI -5.270 to 6.950; Low certainty).
1 finding from 1 review
Immediate (24 h) resin-dentin bond strength (MPa) · Artificial caries-affected dentin (ACAD) in extracted permanent human teeth (in vitro)
In the Self-Etch adhesive + chemical ACAD protocol network, HAp vs Silica showed no significant difference in 24 h bond strength (MD -3.756, 95% CI -10.536 to 3.024; Moderate certainty).
1 finding from 1 review
Immediate (24 h) resin-dentin bond strength (MPa) · permanent human teeth with artificial caries-affected dentin
Calcium minus Fluorine was -0.628 MPa (95% CI -8.504 to 7.248) at 24 h.
1 finding from 1 review
Immediate (24 h) resin-dentin bond strength (MPa) · Artificial caries-affected dentin (ACAD) in extracted permanent human teeth (in vitro)
In the Self-Etch adhesive + chemical ACAD protocol network, HAp showed 4.455 MPa lower 24 h bond strength than Calcium Phosphate (MD -4.455, 95% CI -8.857 to -0.053; Moderate certainty).
2 findings from 1 review
Immediate (24 h) resin-dentin bond strength (MPa) · Artificial caries-affected dentin (ACAD) in extracted permanent human teeth (in vitro)
In the Etch-and-Rinse adhesive + biological ACAD protocol network, Peptide showed 9.857 MPa higher 24 h bond strength than Flavonoids (MD 9.857, 95% CI 2.588 to 17.126; Moderate certainty).
2 findings from 1 review
Immediate (24 h) resin-dentin bond strength (MPa) · Artificial caries-affected dentin (ACAD) in extracted permanent human teeth (in vitro)
In the Self-Etch adhesive + chemical ACAD protocol network, Silica vs Calcium Phosphate showed no significant difference in 24 h bond strength (MD -0.699, 95% CI -7.633 to 6.234; Moderate certainty).
1 finding from 1 review
Immediate (24 h) resin-dentin bond strength (MPa) · Artificial caries-affected dentin (ACAD) in extracted permanent human teeth (in vitro)
In the Self-Etch adhesive + chemical ACAD protocol network, Calcium Phosphate vs Control showed no significant difference in 24 h bond strength (MD 1.539, 95% CI -1.738 to 4.817; Moderate certainty).
1 finding from 1 review
Immediate (24 h) resin-dentin bond strength (MPa) · Artificial caries-affected dentin (ACAD) in extracted permanent human teeth (in vitro)
In the Self-Etch adhesive + chemical ACAD protocol network, HEMA vs Fluorine showed no significant difference in 24 h bond strength (MD 2.500, 95% CI -2.603 to 7.603; Low certainty).
1 finding from 1 review
Immediate (24 h) resin-dentin bond strength (MPa) · Artificial caries-affected dentin (ACAD) in extracted permanent human teeth (in vitro)
In the Self-Etch adhesive + chemical ACAD protocol network, Flavonoids vs Calcium showed no significant difference in 24 h bond strength (MD 5.728, 95% CI -2.442 to 13.897; Moderate certainty).
1 finding from 1 review
Immediate (24 h) resin-dentin bond strength (MPa) · Artificial caries-affected dentin (ACAD) in extracted permanent human teeth (in vitro)
In the Self-Etch adhesive + chemical ACAD protocol network, HAp showed 7.520 MPa lower 24 h bond strength than Flavonoids (MD -7.520, 95% CI -14.758 to -0.281; Moderate certainty).
1 finding from 1 review
Immediate (24 h) resin-dentin bond strength (MPa) · Artificial caries-affected dentin (ACAD) in extracted permanent human teeth (in vitro)
In the Self-Etch adhesive + chemical ACAD protocol network, Silica vs HEMA showed no significant difference in 24 h bond strength (MD -1.059, 95% CI -9.024 to 6.906; Moderate certainty).
1 finding from 1 review
Immediate (24 h) resin-dentin bond strength (MPa) · Artificial caries-affected dentin (ACAD) in extracted permanent human teeth (in vitro)
In the Self-Etch adhesive + chemical ACAD protocol network, Calcium vs Control showed no significant difference in 24 h bond strength (MD -1.124, 95% CI -5.917 to 3.670; Moderate certainty).
1 finding from 1 review