Mesoporous silica (SiO2) vs Calcium phosphate agent (e.g., CPP-ACP, Ca/P-PILP, niobophosphate)
Immediate (24 h) resin-dentin bond strength (MPa) · Artificial caries-affected dentin (ACAD) in extracted permanent human teeth (in vitro)
In the Self-Etch adhesive + chemical ACAD protocol network, Silica vs Calcium Phosphate showed no significant difference in 24 h bond strength (MD -0.699, 95% CI -7.633 to 6.234; Moderate certainty).
1 finding from 1 review
- Biomimetic Remineralization Strategies for Dentin Bond Stability-Systematic Review and Network Meta-Analysis. 2025 All outcomes24 h (immediate) · In vitro; extracted permanent human teeth; bond strength testing (SBS/microSBS/microTBS) · Self-Etch + chemical ACADMD -0.699 [-7.633, 6.234]0 studiesModerate