Search

What do systematic reviews say?

Refine by population, intervention, comparison or outcome
More filters
Evidence found and GRADE certainty

7 questions · 11 findings · 1 reviews · Dental caries

No studies found 0 · 0%GRADE not reported 0 · 0%Very low 0 · 0%Low 5 · 45.5%Moderate 6 · 54.5%High 0 · 0%

Hydroxyapatite (e.g., nano-HAp) vs Calcium-based agent

Immediate (24 h) resin-dentin bond strength (MPa) · Artificial caries-affected dentin (ACAD) in extracted permanent human teeth (in vitro)

In the Self-Etch adhesive + chemical ACAD protocol network, HAp vs Calcium showed no significant difference in 24 h bond strength (MD -1.792, 95% CI -7.415 to 3.831; Low certainty).

2 findings from 1 review

Hydroxyapatite (e.g., nano-HAp) vs HEMA/EGDMA-based desensitizer

Immediate (24 h) resin-dentin bond strength (MPa) · Artificial caries-affected dentin (ACAD) in extracted permanent human teeth (in vitro)

In the Self-Etch adhesive + chemical ACAD protocol network, HAp vs HEMA showed no significant difference in 24 h bond strength (MD -4.815, 95% CI -10.709 to 1.079; Moderate certainty).

1 finding from 1 review

Hydroxyapatite (e.g., nano-HAp) vs No biomimetic remineralization (control)

Immediate (24 h) resin-dentin bond strength (MPa) · Artificial caries-affected dentin (ACAD) in extracted permanent human teeth (in vitro)

In the Self-Etch adhesive + chemical ACAD protocol network, HAp vs Control showed no significant difference in 24 h bond strength (MD -2.916, 95% CI -5.854 to 0.023; Moderate certainty).

2 findings from 1 review

Hydroxyapatite (e.g., nano-HAp) vs Fluoride agent (e.g., NaF/SDF/KF/CaF2)

Immediate (24 h) resin-dentin bond strength (MPa) · Artificial caries-affected dentin (ACAD) in extracted permanent human teeth (in vitro)

In the Etch-and-Rinse adhesive + chemical ACAD protocol network, HAp vs Fluorine showed no significant difference in 24 h bond strength (MD 4.960, 95% CI -1.806 to 11.727; Low certainty).

2 findings from 1 review

Hydroxyapatite (e.g., nano-HAp) vs Mesoporous silica (SiO2)

Immediate (24 h) resin-dentin bond strength (MPa) · Artificial caries-affected dentin (ACAD) in extracted permanent human teeth (in vitro)

In the Self-Etch adhesive + chemical ACAD protocol network, HAp vs Silica showed no significant difference in 24 h bond strength (MD -3.756, 95% CI -10.536 to 3.024; Moderate certainty).

1 finding from 1 review

Hydroxyapatite (e.g., nano-HAp) vs Calcium phosphate agent (e.g., CPP-ACP, Ca/P-PILP, niobophosphate)

Immediate (24 h) resin-dentin bond strength (MPa) · Artificial caries-affected dentin (ACAD) in extracted permanent human teeth (in vitro)

In the Self-Etch adhesive + chemical ACAD protocol network, HAp showed 4.455 MPa lower 24 h bond strength than Calcium Phosphate (MD -4.455, 95% CI -8.857 to -0.053; Moderate certainty).

2 findings from 1 review

Hydroxyapatite (e.g., nano-HAp) vs Flavonoids (e.g., quercetin, proanthocyanidin)

Immediate (24 h) resin-dentin bond strength (MPa) · Artificial caries-affected dentin (ACAD) in extracted permanent human teeth (in vitro)

In the Self-Etch adhesive + chemical ACAD protocol network, HAp showed 7.520 MPa lower 24 h bond strength than Flavonoids (MD -7.520, 95% CI -14.758 to -0.281; Moderate certainty).

1 finding from 1 review