Immediate (24 h) resin-dentin bond strength (MPa) · Artificial caries-affected dentin (ACAD) in extracted permanent human teeth (in vitro)
In the Self-Etch adhesive + chemical ACAD protocol network, Silica vs Fluorine showed no significant difference in 24 h bond strength (MD 1.441, 95% CI -5.099 to 7.980; Moderate certainty).
1 finding from 1 review
Immediate (24 h) resin-dentin bond strength (MPa) · Artificial caries-affected dentin (ACAD) in extracted permanent human teeth (in vitro)
In the Etch-and-Rinse adhesive + biological ACAD protocol network, Flavonoids vs Fluorine showed no significant difference in 24 h bond strength (MD 4.241, 95% CI -2.652 to 11.135; Moderate certainty).
2 findings from 1 review
Immediate (24 h) resin-dentin bond strength (MPa) · Artificial caries-affected dentin (ACAD) in extracted permanent human teeth (in vitro)
In the Self-Etch adhesive + chemical ACAD protocol network, Peptide vs Calcium Phosphate showed no significant difference in 24 h bond strength (MD -0.009, 95% CI -4.076 to 4.058; Low certainty).
3 findings from 1 review
Immediate (24 h) resin-dentin bond strength (MPa) · Artificial caries-affected dentin (ACAD) in extracted permanent human teeth (in vitro)
In the Self-Etch adhesive + chemical ACAD protocol network, HEMA vs Control showed no significant difference in 24 h bond strength (MD 1.899, 95% CI -3.210 to 7.009; Low certainty).
1 finding from 1 review
Immediate (24 h) resin-dentin bond strength (MPa) · Artificial caries-affected dentin (ACAD) in extracted permanent human teeth (in vitro)
In the Self-Etch adhesive + chemical ACAD protocol network, Peptide vs Calcium showed no significant difference in 24 h bond strength (MD 2.654, 95% CI -3.216 to 8.524; Moderate certainty).
2 findings from 1 review
Immediate (24 h) resin-dentin bond strength (MPa) · Artificial caries-affected dentin (ACAD) in extracted permanent human teeth (in vitro)
In the Self-Etch adhesive + chemical ACAD protocol network, Silica vs Calcium showed no significant difference in 24 h bond strength (MD 1.964, 95% CI -5.802 to 9.730; Moderate certainty).
1 finding from 1 review
Immediate (24 h) resin-dentin bond strength (MPa) · Artificial caries-affected dentin (ACAD) in extracted permanent human teeth (in vitro)
In the Self-Etch adhesive + chemical ACAD protocol network, Peptide vs Fluorine showed no significant difference in 24 h bond strength (MD 2.131, 95% CI -2.213 to 6.475; Low certainty).
3 findings from 1 review
Immediate (24 h) resin-dentin bond strength (MPa) · Artificial caries-affected dentin (ACAD) in extracted permanent human teeth (in vitro)
In the Self-Etch adhesive + chemical ACAD protocol network, Peptide vs Control showed no significant difference in 24 h bond strength (MD 1.530, 95% CI -2.373 to 5.434; Moderate certainty).
3 findings from 1 review
Immediate (24 h) resin-dentin bond strength (MPa) · Artificial caries-affected dentin (ACAD) in extracted permanent human teeth (in vitro)
In the Etch-and-Rinse adhesive + chemical ACAD protocol network, Peptide vs HAp showed no significant difference in 24 h bond strength (MD -0.288, 95% CI -7.988 to 7.411; Very Low certainty).
2 findings from 1 review
Immediate (24 h) resin-dentin bond strength (MPa) · permanent human teeth with artificial caries-affected dentin
Peptide minus Silica was -0.690 MPa (95% CI -7.941 to 6.560) at 24 h.
1 finding from 1 review
Immediate (24 h) resin-dentin bond strength (MPa) · Artificial caries-affected dentin (ACAD) in extracted permanent human teeth (in vitro)
In the Etch-and-Rinse adhesive + biological ACAD protocol network, Flavonoids showed 12.771 MPa lower 24 h bond strength than Calcium Phosphate (MD -12.771, 95% CI -20.538 to -5.003; Moderate certainty).
2 findings from 1 review
Immediate (24 h) resin-dentin bond strength (MPa) · Artificial caries-affected dentin (ACAD) in extracted permanent human teeth (in vitro)
In the Etch-and-Rinse adhesive + biological ACAD protocol network, Flavonoids showed 8.438 MPa higher 24 h bond strength than Control (MD 8.438, 95% CI 2.289 to 14.587; Moderate certainty).
2 findings from 1 review
Immediate (24 h) resin-dentin bond strength (MPa) · Artificial caries-affected dentin (ACAD) in extracted permanent human teeth (in vitro)
In the Self-Etch adhesive + chemical ACAD protocol network, HEMA vs Calcium showed no significant difference in 24 h bond strength (MD 3.023, 95% CI -3.815 to 9.861; Moderate certainty).
1 finding from 1 review
Immediate (24 h) resin-dentin bond strength (MPa) · Artificial caries-affected dentin (ACAD) in extracted permanent human teeth (in vitro)
In the Self-Etch adhesive + chemical ACAD protocol network, Peptide vs HEMA showed no significant difference in 24 h bond strength (MD -0.369, 95% CI -6.728 to 5.990; Low certainty).
1 finding from 1 review
Immediate (24 h) resin-dentin bond strength (MPa) · Artificial caries-affected dentin (ACAD) in extracted permanent human teeth (in vitro)
In the Self-Etch adhesive + chemical ACAD protocol network, HEMA vs Calcium Phosphate showed no significant difference in 24 h bond strength (MD 0.360, 95% CI -5.589 to 6.309; Moderate certainty).
1 finding from 1 review
Immediate (24 h) resin-dentin bond strength (MPa) · Artificial caries-affected dentin (ACAD) in extracted permanent human teeth (in vitro)
In the Self-Etch adhesive + chemical ACAD protocol network, Flavonoids vs HEMA showed no significant difference in 24 h bond strength (MD 2.705, 95% CI -5.654 to 11.063; Moderate certainty).
1 finding from 1 review
Immediate (24 h) resin-dentin bond strength (MPa) · Artificial caries-affected dentin (ACAD) in extracted permanent human teeth (in vitro)
In the Self-Etch adhesive + chemical ACAD protocol network, Silica vs Control showed no significant difference in 24 h bond strength (MD 0.840, 95% CI -5.270 to 6.950; Low certainty).
1 finding from 1 review
Immediate (24 h) resin-dentin bond strength (MPa) · Artificial caries-affected dentin (ACAD) in extracted permanent human teeth (in vitro)
In the Etch-and-Rinse adhesive + biological ACAD protocol network, Peptide showed 9.857 MPa higher 24 h bond strength than Flavonoids (MD 9.857, 95% CI 2.588 to 17.126; Moderate certainty).
2 findings from 1 review
Immediate (24 h) resin-dentin bond strength (MPa) · Artificial caries-affected dentin (ACAD) in extracted permanent human teeth (in vitro)
In the Self-Etch adhesive + chemical ACAD protocol network, Silica vs Calcium Phosphate showed no significant difference in 24 h bond strength (MD -0.699, 95% CI -7.633 to 6.234; Moderate certainty).
1 finding from 1 review
Immediate (24 h) resin-dentin bond strength (MPa) · Artificial caries-affected dentin (ACAD) in extracted permanent human teeth (in vitro)
In the Self-Etch adhesive + chemical ACAD protocol network, HEMA vs Fluorine showed no significant difference in 24 h bond strength (MD 2.500, 95% CI -2.603 to 7.603; Low certainty).
1 finding from 1 review