No studies found 0 · 0%GRADE not reported 0 · 0%Very low 1 · 6.3%Low 5 · 31.3%Moderate 10 · 62.5%High 0 · 0%

Self-assembling/remineralizing peptide (e.g., P11-4, PAA-PASP) vs Calcium phosphate agent (e.g., CPP-ACP, Ca/P-PILP, niobophosphate)

Immediate (24 h) resin-dentin bond strength (MPa) · Artificial caries-affected dentin (ACAD) in extracted permanent human teeth (in vitro)

In the Self-Etch adhesive + chemical ACAD protocol network, Peptide vs Calcium Phosphate showed no significant difference in 24 h bond strength (MD -0.009, 95% CI -4.076 to 4.058; Low certainty).

3 findings from 1 review

Self-assembling/remineralizing peptide (e.g., P11-4, PAA-PASP) vs Calcium-based agent

Immediate (24 h) resin-dentin bond strength (MPa) · Artificial caries-affected dentin (ACAD) in extracted permanent human teeth (in vitro)

In the Self-Etch adhesive + chemical ACAD protocol network, Peptide vs Calcium showed no significant difference in 24 h bond strength (MD 2.654, 95% CI -3.216 to 8.524; Moderate certainty).

2 findings from 1 review

Self-assembling/remineralizing peptide (e.g., P11-4, PAA-PASP) vs Fluoride agent (e.g., NaF/SDF/KF/CaF2)

Immediate (24 h) resin-dentin bond strength (MPa) · Artificial caries-affected dentin (ACAD) in extracted permanent human teeth (in vitro)

In the Self-Etch adhesive + chemical ACAD protocol network, Peptide vs Fluorine showed no significant difference in 24 h bond strength (MD 2.131, 95% CI -2.213 to 6.475; Low certainty).

3 findings from 1 review

Self-assembling/remineralizing peptide (e.g., P11-4, PAA-PASP) vs No biomimetic remineralization (control)

Immediate (24 h) resin-dentin bond strength (MPa) · Artificial caries-affected dentin (ACAD) in extracted permanent human teeth (in vitro)

In the Self-Etch adhesive + chemical ACAD protocol network, Peptide vs Control showed no significant difference in 24 h bond strength (MD 1.530, 95% CI -2.373 to 5.434; Moderate certainty).

3 findings from 1 review

Self-assembling/remineralizing peptide (e.g., P11-4, PAA-PASP) vs Hydroxyapatite (e.g., nano-HAp)

Immediate (24 h) resin-dentin bond strength (MPa) · Artificial caries-affected dentin (ACAD) in extracted permanent human teeth (in vitro)

In the Etch-and-Rinse adhesive + chemical ACAD protocol network, Peptide vs HAp showed no significant difference in 24 h bond strength (MD -0.288, 95% CI -7.988 to 7.411; Very Low certainty).

2 findings from 1 review

Self-assembling/remineralizing peptide (e.g., P11-4, PAA-PASP) vs HEMA/EGDMA-based desensitizer

Immediate (24 h) resin-dentin bond strength (MPa) · Artificial caries-affected dentin (ACAD) in extracted permanent human teeth (in vitro)

In the Self-Etch adhesive + chemical ACAD protocol network, Peptide vs HEMA showed no significant difference in 24 h bond strength (MD -0.369, 95% CI -6.728 to 5.990; Low certainty).

1 finding from 1 review

Self-assembling/remineralizing peptide (e.g., P11-4, PAA-PASP) vs Flavonoids (e.g., quercetin, proanthocyanidin)

Immediate (24 h) resin-dentin bond strength (MPa) · Artificial caries-affected dentin (ACAD) in extracted permanent human teeth (in vitro)

In the Etch-and-Rinse adhesive + biological ACAD protocol network, Peptide showed 9.857 MPa higher 24 h bond strength than Flavonoids (MD 9.857, 95% CI 2.588 to 17.126; Moderate certainty).