Question · asked by 1 review

Metal-reinforced glass-ionomer cement (MRGIC) restoration vs Conventional GIC: Treatment failure (annual failure rate)

Population
Children with previously unrestored, vital carious lesions in primary teeth (no pulp therapy); aged 1.5-11 years
Intervention
Metal-reinforced glass-ionomer cement (MRGIC) restoration
Comparison
Conventional GIC
Outcome
Treatment failure (annual failure rate)

Metal-reinforced GIC had a high annual failure rate (29.9%) in a single RCT; low quality of evidence (ungraded).

What each review found

Include earlier review versions
FindingEffectStudiesGRADE certainty
Metal-reinforced glass-ionomer cement (MRGIC) restoration vs Conventional GIC
Treatment failure (annual failure rate) · Children with previously unrestored, vital carious lesions in primary teeth (no pulp therapy); aged 1.5-11 years · 1.5 years mean follow-up (Kilpatrick 1995), Not reported (UK)
Metal-reinforced GIC had a high annual failure rate (29.9%) in a single RCT; low quality of evidence (ungraded).
Clinical effectiveness of restorative materials for the restoration of carious primary teeth without pulp… (2022) All outcomes
Annual failure rate (%) 29.91 study · 37 participantsGRADE not reported

Findings are shown side by side, never pooled across reviews.

The reviews

Studies behind the findings

The primary studies the full-text reviews tie to this outcome. Reviews with headline outcomes only do not list them here.

How reviews are matched to this question

Reviews word the same question differently. Four decision models (TypeSafe's Jev, Liquid AI's d1-ultra, SubQ Snap and Baseten's Elephant) judged each wording of the population, intervention, comparator and outcome against the others; two wordings count as the same when at least three of them agree and none clearly disagrees, and findings count as this question only when all four elements match. Timing, setting and subgroup never split a question: they are shown on each finding.